Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite

Category Ceramic , Oxide , Aluminum Oxide , Metal , Metal Matrix Composite , Nonferrous Metal , Aluminum Alloy
Manufacturer Metal Matrix Cast Composites (MMCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cast, reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Physical Properties Metric English Comments
Density 3.50 g/cc
0.126 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1200 - 1400 MPa
174000 - 203000 psi
Modulus of Elasticity 290 - 310 GPa
42100 - 45000 ksi
Youngs Modulus
Thermal Properties Metric English Comments
CTE, linear 10.0 - 12.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 6.67 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved