Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 3.60 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.60 GPa
522 ksi
dry
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
Modulus of Elasticity 3.60 GPa
522 ksi
Lehmann & Voss LUVOCOM® 1105-7786 PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Emergency running property.Improved wear behaviour, low warpage.High chemical resistance p..
Modulus of Elasticity 3.60 GPa
522 ksi
Lehmann & Voss LUVOCOM® 1105-7685 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Super..
Modulus of Elasticity 3.60 GPa
522 ksi
TD; ExxonMobil Method
ExxonMobil Bicor™ 18MB090 OPP Film
Product Description: Biaxially oriented polypropylene film metallizable on one side, with a slip controlled broad seal range surface on the other side. Once metalized, film designed to be used in la..
Modulus of Elasticity 3.60 GPa
522 ksi
TD; ExxonMobil Method
ExxonMobil Bicor™ 20MB080 OPP Film
Product Description: Bicor 20NB080 is a biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a s..
Modulus of Elasticity 3.60 GPa
522 ksi
TD; ExxonMobil Method
ExxonMobil Bicor™ 29MB080 OPP Film
Product Description: A biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a single web in HFFS..
Modulus of Elasticity 3.60 GPa
522 ksi
TD; ExxonMobil Method
ExxonMobil Label-Lyte™ 29LL210 Preliminary Data Sheet OPP Film
Product Description: A biaxially oriented, transparent polypropylene film for pressure sensitive labeling and tape applications.Availability: Africa & Middle East and EuropeKey Features: High yieldG..
Modulus of Elasticity 3.60 GPa
522 ksi
TD; ExxonMobil Method
ExxonMobil Metallyte™ 18MM383 OPP Film
Product Description: A biaxially oriented very high barrier metalized polypropylene film. This film offers an outstanding moisture barrier and a broad seal range surface on the other side. This film..
Modulus of Elasticity 3.60 GPa
522 ksi
TD; ExxonMobil Method
ExxonMobil Metallyte™ 18MM388 OPP Film
Product Description: A metallized biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance p..
Modulus of Elasticity 3.60 GPa
522 ksi
TD; ExxonMobil Method
ExxonMobil Metallyte™ 18MM488 OPP Film
Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c..
Modulus of Elasticity 3.60 GPa
522 ksi
TD; ExxonMobil Method
ExxonMobil Metallyte™ 20MM480 OPP Film
Product Description: A metalized biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. It is typically used in lamination with other substrates on HFFS and V..
Modulus of Elasticity 3.60 GPa
522 ksi
ISO 527-1/-2
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned)
Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for..
Modulus of Elasticity 3.60 GPa
522 ksi
ISO 527-1/-2
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry)
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector..
Modulus of Elasticity 3.60 GPa
522 ksi
ISO 527-1/-2
BASF Ultramid® C3U10 PA6/66 FR (Dry)
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector..
Modulus of Elasticity 3.60 GPa
522 ksi
ISO 178
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead
Flame retardant, 15% glass bead filled, with halogensInformation provided by Addiplast.