Mechanical Properties Metric English Comments
Modulus of Elasticity 10.0 - 30.0 GPa
1450 - 4350 ksi
After Sintering
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative
NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package..
Modulus of Elasticity 9.50 - 30.0 GPa
1380 - 4350 ksi
Average value: 18.7 GPa Grade Count:19
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Modulus of Elasticity 6.00 - 30.0 GPa
870 - 4350 ksi
Average value: 16.4 GPa Grade Count:31
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..