Polymer Property : Modulus of Elasticity = 3020 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 5.80 - 20.8 GPa
841 - 3020 ksi
Average value: 10.4 GPa Grade Count:16
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..