Mechanical Properties Metric English Comments
Modulus of Elasticity 5.80 - 20.8566 GPa

@Temperature -40.0 - 150 °C
841 - 3025.05 ksi

@Temperature -40.0 - 302 °F
Average value: 11.8 GPa Grade Count:4
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
Modulus of Elasticity 5.80 GPa
841 ksi
ISO 527-2
Tisan TISOPLEN® 30% Glass Fiber Filled Reinforced Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Modulus of Elasticity 5.80 GPa
841 ksi
Conditioned; ISO 178
Addiplast Addinyl A2 V30 Nylon 66, 30% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 5.80 GPa
841 ksi
Conditioned; ISO 178
Addiplast Addinyl A2 ZV30 Nylon 66, 30% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 5.80 GPa
841 ksi
ISO 527-1/-2
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
Modulus of Elasticity 5.80 GPa
841 ksi
ISO 527-1/-2
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
Modulus of Elasticity 5.80 GPa
841 ksi
ISO 527-1/-2
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
Modulus of Elasticity 5.80 - 20.8 GPa
841 - 3020 ksi
Average value: 10.4 GPa Grade Count:16