Polymer Property : Modulus of Elasticity = 307.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.117 GPa
307.0 ksi
ASTM D638M
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure  (discontinued **)
DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..