Mechanical Properties Metric English Comments
Modulus of Elasticity 2.193 - 17.1 GPa

@Temperature -40.0 - 150 °C
318.1 - 2480 ksi

@Temperature -40.0 - 302 °F
Average value: 8.31 GPa Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..