Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 40% Glass Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.48 - 1.79 g/cc
0.0535 - 0.0647 lb/in³
Average value: 1.64 g/cc Grade Count:22
1.32 - 1.32 g/cc

@Temperature 285 - 285 °C
0.0477 - 0.0477 lb/in³

@Temperature 545 - 545 °F
Average value: 1.32 g/cc Grade Count:1
Filler Content 35.0 - 43.0 %
35.0 - 43.0 %
Average value: 39.5 % Grade Count:4
Water Absorption 0.0400 - 0.830 %
0.0400 - 0.830 %
Average value: 0.373 % Grade Count:14
Moisture Absorption at Equilibrium 0.130 - 0.240 %
0.130 - 0.240 %
Average value: 0.178 % Grade Count:10
Viscosity 12500 - 250000 cP

@Temperature 270 - 310 °C
12500 - 250000 cP

@Temperature 518 - 590 °F
Average value: 96700 cP Grade Count:1
12500 - 250000 cP

@Shear Rate 100 - 100000 1/s
12500 - 250000 cP

@Shear Rate 100 - 100000 1/s
Average value: 96700 cP Grade Count:1
Linear Mold Shrinkage 0.000500 - 0.00650 cm/cm
0.000500 - 0.00650 in/in
Average value: 0.00282 cm/cm Grade Count:15
Linear Mold Shrinkage, Transverse 0.00500 - 0.0105 cm/cm
0.00500 - 0.0105 in/in
Average value: 0.00819 cm/cm Grade Count:12
Melt Flow 6.00 - 20.0 g/10 min
6.00 - 20.0 g/10 min
Average value: 12.1 g/10 min Grade Count:4
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115 - 122
115 - 122
Average value: 119 Grade Count:4
Tensile Strength, Ultimate 31.0 - 207 MPa
4500 - 30000 psi
Average value: 144 MPa Grade Count:20
55.2 - 210 MPa

@Temperature -40.0 - 150 °C
8010 - 30500 psi

@Temperature -40.0 - 302 °F
Average value: 87.1 MPa Grade Count:1
22.4 - 200 MPa

@Temperature -40.0 - 150 °C
3250 - 29000 psi

@Temperature -40.0 - 302 °F
Average value: 87.1 MPa Grade Count:1
22.4 - 200 MPa

@Strain 0.140 - 4.69 %
3250 - 29000 psi

@Strain 0.140 - 4.69 %
Average value: 87.1 MPa Grade Count:1
Elongation at Break 1.00 - 3.60 %
1.00 - 3.60 %
Average value: 2.22 % Grade Count:19
1.70 - 5.50 %

@Temperature -40.0 - 150 °C
1.70 - 5.50 %

@Temperature -40.0 - 302 °F
Average value: 3.83 % Grade Count:1
Modulus of Elasticity 6.90 - 17.0 GPa
1000 - 2470 ksi
Average value: 12.9 GPa Grade Count:18
2.193 - 17.1 GPa

@Temperature -40.0 - 150 °C
318.1 - 2480 ksi

@Temperature -40.0 - 302 °F
Average value: 8.31 GPa Grade Count:2
Flexural Yield Strength 132 - 269 MPa
19100 - 39000 psi
Average value: 209 MPa Grade Count:8
79.3 - 310 MPa

@Temperature -40.0 - 150 °C
11500 - 45000 psi

@Temperature -40.0 - 302 °F
Average value: 176 MPa Grade Count:1
Flexural Modulus 7.52 - 14.5 GPa
1090 - 2100 ksi
Average value: 10.7 GPa Grade Count:10
2.90 - 15.2 GPa

@Temperature -40.0 - 150 °C
421 - 2200 ksi

@Temperature -40.0 - 302 °F
Average value: 8.35 GPa Grade Count:1
Compressive Yield Strength 172 - 231 MPa
25000 - 33500 psi
Average value: 192 MPa Grade Count:3
Shear Modulus >= 0.0920 GPa

@Temperature -50.0 - 250 °C
>= 13.3 ksi

@Temperature -58.0 - 482 °F
Average value: 1.64 GPa Grade Count:2
Izod Impact, Notched 0.801 - 1.28 J/cm
1.50 - 2.40 ft-lb/in
Average value: 0.949 J/cm Grade Count:7
0.910 - 0.910 J/cm

@Temperature -40.0 - -40.0 °C
1.70 - 1.70 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.910 J/cm Grade Count:1
Izod Impact, Unnotched 6.41 - 8.54 J/cm
12.0 - 16.0 ft-lb/in
Average value: 7.35 J/cm Grade Count:4
5.10 - 5.10 J/cm

@Temperature -40.0 - -40.0 °C
9.55 - 9.55 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 5.10 J/cm Grade Count:1
Charpy Impact Unnotched 2.10 - 6.50 J/cm²
9.99 - 30.9 ft-lb/in²
Average value: 4.59 J/cm² Grade Count:15
2.00 - 6.00 J/cm²

@Temperature -40.0 - -30.0 °C
9.52 - 28.6 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.35 J/cm² Grade Count:9
Charpy Impact, Notched 0.340 - 1.20 J/cm²
1.62 - 5.71 ft-lb/in²
Average value: 0.851 J/cm² Grade Count:14
0.400 - 1.20 J/cm²

@Temperature -40.0 - -30.0 °C
1.90 - 5.71 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.850 J/cm² Grade Count:9
Thermal Properties Metric English Comments
CTE, linear 16.0 - 500 µm/m-°C
8.89 - 278 µin/in-°F
Average value: 183 µm/m-°C Grade Count:12
500 - 500 µm/m-°C

@Temperature 55.0 - 160 °C
278 - 278 µin/in-°F

@Temperature 131 - 320 °F
Average value: 500 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 40.0 - 85.0 µm/m-°C
22.2 - 47.2 µin/in-°F
Average value: 61.8 µm/m-°C Grade Count:10
96.0 - 96.0 µm/m-°C

@Temperature 55.0 - 160 °C
53.3 - 53.3 µin/in-°F

@Temperature 131 - 320 °F
Average value: 96.0 µm/m-°C Grade Count:1
Thermal Conductivity 0.303 - 1.65 W/m-K
2.10 - 11.5 BTU-in/hr-ft²-°F
Average value: 0.675 W/m-K Grade Count:4
Melting Point 246 - 255 °C
475 - 491 °F
Average value: 252 °C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 232 - 250 °C
450 - 482 °F
Average value: 245 °C Grade Count:13
Deflection Temperature at 1.8 MPa (264 psi) 200 - 248 °C
392 - 478 °F
Average value: 227 °C Grade Count:18
Flammability, UL94 HB - 5VA
HB - 5VA
Grade Count:16
Electrical Properties Metric English Comments
Electrical Resistivity 3.00e+13 - 1.00e+16 ohm-cm
3.00e+13 - 1.00e+16 ohm-cm
Average value: 3.00e+15 ohm-cm Grade Count:12
Surface Resistance 1.00e+13 - 1.00e+15 ohm
1.00e+13 - 1.00e+15 ohm
Average value: 6.85e+14 ohm Grade Count:5
Dielectric Constant 3.10 - 125
3.10 - 125
Average value: 14.7 Grade Count:11
Dielectric Strength 1.10 - 39.0 kV/mm
27.9 - 991 kV/in
Average value: 26.4 kV/mm Grade Count:12
12.0 - 21.5 kV/mm

@Temperature 95.0 - 150 °C
305 - 546 kV/in

@Temperature 203 - 302 °F
Average value: 15.8 kV/mm Grade Count:1
12.0 - 21.5 kV/mm

@Thickness 1.60 - 3.20 mm
305 - 546 kV/in

@Thickness 0.0630 - 0.126 in
Average value: 15.8 kV/mm Grade Count:1
Dissipation Factor 0.00300 - 0.0300
0.00300 - 0.0300
Average value: 0.0109 Grade Count:9
Comparative Tracking Index 250 - 400 V
250 - 400 V
Average value: 265 V Grade Count:8
Users viewing this material also viewed the following: