Mechanical Properties Metric English Comments
Modulus of Elasticity 340 GPa
49300 ksi
Plansee DENSIMET® D170 Tungsten-Nickel-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..
Modulus of Elasticity 340 GPa
49300 ksi
H.C. Starck HPM 1750 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Modulus of Elasticity 340 GPa
49300 ksi
H.C. Starck HPM 1760 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Modulus of Elasticity 340 GPa
49300 ksi
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Modulus of Elasticity 340 GPa
49300 ksi
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet
Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo..
Modulus of Elasticity 340 GPa
49300 ksi
ASTM-F417
CeramTec CeramCool® Rubalit® 708 Alumina, 96%
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..
Modulus of Elasticity 340 GPa
49300 ksi
DIN V ENV 843-2
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance)
Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn..