Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 340 GPa | 49300 ksi | |
Plansee DENSIMET® D170 Tungsten-Nickel-Iron Alloy Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d.. |
|||
Modulus of Elasticity | 340 GPa | 49300 ksi | |
H.C. Starck HPM 1750 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Modulus of Elasticity | 340 GPa | 49300 ksi | |
H.C. Starck HPM 1760 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Modulus of Elasticity | 340 GPa | 49300 ksi | |
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
Modulus of Elasticity | 340 GPa | 49300 ksi | |
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo.. |
|||
Modulus of Elasticity | 340 GPa | 49300 ksi | ASTM-F417 |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
Modulus of Elasticity | 340 GPa | 49300 ksi | DIN V ENV 843-2 |
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance) Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn.. |