Polymer Property : Modulus of Elasticity = 36.3 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.250 GPa
36.3 ksi
TD; ISO R527-1
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene
LDPE 2404TC47 Light duty FilmIt is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.Information provi..
Modulus of Elasticity 0.250 GPa
36.3 ksi
MD; ISO 527
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene
LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p..
Modulus of Elasticity 0.250 GPa
36.3 ksi
ISO 527-2
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating
LDPE LA 0304 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum.Information provided by Total Pe..