Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer Total Atofina
Trade Name LDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LDPE LA 0304 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.924 g/cc
0.924 g/cc
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
ISO 527-2
Tensile Strength, Yield 11.0 MPa
1600 psi
ISO 527-2
Elongation at Break 550 %
550 %
ISO 527-2
Modulus of Elasticity 0.250 GPa
36.3 ksi
ISO 527-2
Thermal Properties Metric English Comments
Melting Point 111 °C
232 °F
ISO 11357
Vicat Softening Point 95.0 °C
203 °F
ISO 306
Processing Properties Metric English Comments
Processing Temperature 200 - 320 °C
392 - 608 °F
Melt Temperature 260 - 320 °C
500 - 608 °F
Die Melt Temp