Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.55 - 26.7 GPa @Temperature 60.0 - 150 °C |
370 - 3870 ksi @Temperature 140 - 302 °F |
Average value: 20.0 GPa Grade Count:4 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Modulus of Elasticity | 2.55 GPa | 370 ksi | ASTM D638 |
Ineos Nova 4211 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Modulus of Elasticity | 2.55 GPa | 370 ksi | DIN 53457 |
Ineos Nova S-5100 High Impact Compact Polystyrene
(discontinued **) All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture betwee.. |
|||
Modulus of Elasticity | 2.55 - 2.82 GPa | 370 - 409 ksi | Average value: 2.70 GPa Grade Count:8 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Modulus of Elasticity | 2.55 GPa | 370 ksi | Secant; ASTM D5026 |
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4.. |
|||
Modulus of Elasticity | 2.55 - 2.93 GPa @Temperature 22.8 °C |
370 - 425 ksi @Temperature 73.0 °F |
|
Ensinger TECAST VEKTON™ 6PB Nylon 6 (PA6) TECAST VEKTON™ 6PB cushion pads are used to dampen the shock load on the anvil of a pile hammer. Specially formulated from an impact-modified type 6 nylon, they combine the excellent strength of n.. |
|||
Modulus of Elasticity | 2.55 - 7.00 GPa | 370 - 1020 ksi | Average value: 5.73 GPa Grade Count:12 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Modulus of Elasticity | 2.55 GPa | 370 ksi | ASTM D638 |
GEHR Plastics Noryl PPO
(discontinued **) PPO belongs to the group of the amorphous materials and can be used in temperatures ranging from -58 °F to +302 °F. PPO exhibits a high impact strength and a very high dimensional stability. The e.. |