Mechanical Properties Metric English Comments
Modulus of Elasticity 0.290 GPa
42.1 ksi
Secant; ASTM D638
Huntsman PE5030 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa..
Modulus of Elasticity 0.290 GPa
42.1 ksi
Secant; ASTM D638
Huntsman PE5032 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, excellent heat sealability, good adhesion, low smoking, no edge weave, and excellent printability.Applications: Extrusion: c..
Modulus of Elasticity 0.290 GPa
42.1 ksi
Secant; ASTM D638
Huntsman PE1155 EVA Film Extrusion  (discontinued **)
1.5% Vinyl Acetate EVA Copolymer and FDA compliant.Features: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications:..