Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 30.0 GPa | 4350 ksi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass Epoxies are highly resistant to water, alkalis and organic solvents. Although standard epoxies have only a fair resistance to acids and oxidizing agents, they can be formulated for better resistance.. |
|||
Modulus of Elasticity | 30.0 GPa | 4350 ksi | |
Lehmann & Voss LUVOCOM® 20/XCF/30 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Modulus of Elasticity | 30.0 GPa | 4350 ksi | |
Lehmann & Voss LUVOCOM® 20-0916 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Modulus of Elasticity | 30.0 GPa | 4350 ksi | |
Indium Corp. Indalloy 213 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Modulus of Elasticity | 30.0 GPa | 4350 ksi | |
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation. |
|||
Modulus of Elasticity | 30.0 GPa | 4350 ksi | |
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Modulus of Elasticity | 30.0 GPa | 4350 ksi | |
Lehmann & Voss LUVOCOM® 1105-7536 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Modulus of Elasticity | 30.0 GPa | 4350 ksi | |
Indium Corp. Indalloy 109 Tin-Lead Solder Alloy Good electrical grade solderInformation Provided by Indium Corporation |