Material Notes:
Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 8.40 g/cc
0.303 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 17
17
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Elongation at Break 37 %
37 %
Modulus of Elasticity 30.0 GPa
4350 ksi
Shear Strength 42.7 MPa
6190 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.167 J/g-°C
0.0399 BTU/lb-°F
Solid
Thermal Conductivity 50.0 W/m-K

@Temperature 85.0 °C
347 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 183 °C
361 °F
Eutectic
Solidus 183 °C
361 °F
Liquidus 183 °C
361 °F
Component Elements Properties Metric English Comments
Lead, Pb 37 %
37 %
Tin, Sn 63 %
63 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm
Copyright © lookpolymers.com All Rights Reserved