Polymer Property : Modulus of Elasticity = 45000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 310 GPa
45000 ksi
Hogen HM1100 Tungsten-Based Metal
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers hig..
Modulus of Elasticity 310 GPa
45000 ksi
Hogen HM3000 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l..
Modulus of Elasticity 310 GPa
45000 ksi
Mi-Tech Metals HD17D Tungsten-Based Metal
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The t..
Modulus of Elasticity 310 GPa
45000 ksi
Mi-Tech Metals HD18 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm..
Modulus of Elasticity 310 GPa
45000 ksi
ASTM-C623
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate
This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers
Modulus of Elasticity 310 GPa
45000 ksi
ASTM C848
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide
Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Modulus of Elasticity 310 GPa
45000 ksi
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.
Modulus of Elasticity 310 GPa
45000 ksi
Astro Met ZTA 96 Zirconia Toughened Alumina
General Description:ZTA-96 is a zirconia toughened alumina ceramic that exhibits excellent wear and corrosion resistance along with high strength and toughness. Astro Met has developed ZTA-96 zircon..
Modulus of Elasticity 310 GPa
45000 ksi
Ceradyne Ceralloy® 147-31E Sintered Reaction Bonded Silicon Nitride (Si3N4)
Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met..
Modulus of Elasticity 310 GPa
45000 ksi
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)
Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met..
Modulus of Elasticity 310 GPa
45000 ksi
ATI Wah Chang Infiltrated Tungsten (Copper)
Tungsten base infiltrated metal with Copper as infiltrant has been widely used in industry for years. It has proven highly advantageous because of its excellent machinability. Roughly 90% Tungsten a..
Modulus of Elasticity 310 GPa
45000 ksi
Ceradyne Ceralloy® 147-1E Silicon Nitride
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradynes ..
Modulus of Elasticity 310 GPa
45000 ksi
Ceradyne Ceralloy® 147-31N Sintered Reaction Bonded Silicon Nitride (Si3N4)
Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met..
Modulus of Elasticity 310 GPa
45000 ksi
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4)
EKatherm® Silicon Nitride is the state-of-the-art material for a wide variety of components used in Aluminum Alloy casting processes.Features: High Temperature Resistance High Thermal Shock Resist..