CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide

Category Ceramic , Carbide
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.Data Provided by the manufacturer, CoorsTek, Inc.
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
ASTM C20
Water Absorption 0.00 %
0.00 %
ASTM 373
Particle Size 6.0 µm
6.0 µm
Thin Section Crystal Size
Mechanical Properties Metric English Comments
Knoop Microhardness 26
26
1000 g
Modulus of Elasticity 310 GPa
45000 ksi
ASTM C848
Flexural Strength 220 MPa
31900 psi
ASTM F417
Compressive Strength 675 MPa
97900 psi
ASTM C773
Poissons Ratio 0.18
0.18
ASTM C848
Fracture Toughness 3.20 MPa-m½
2.91 ksi-in½
Notched Beam
Shear Modulus 131 GPa
19000 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 4.40 µm/m-°C

@Temperature 25.0 - 1000 °C
2.44 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
Specific Heat Capacity 0.820 J/g-°C
0.196 BTU/lb-°F
ASTM E1269
Thermal Conductivity 125 W/m-K
868 BTU-in/hr-ft²-°F
ASTM C408
Maximum Service Temperature, Air 1600 °C
2910 °F
No Load
Electrical Properties Metric English Comments
Electrical Resistivity <= 1e+05
<= 1e+05
ASTM D1829
<= 1000 ohm-cm

@Temperature 500 °C
<= 1000 ohm-cm

@Temperature 932 °F
ASTM D1829
<= 1000 ohm-cm

@Temperature 1000 °C
<= 1000 ohm-cm

@Temperature 1830 °F
ASTM D1829
Descriptive Properties Value Comments
Color Black