Modulus of Elasticity 2.90 - 5.30 GPa

@Temperature 60.0 - 90.0 °C
421 - 769 ksi

@Temperature 140 - 194 °F
Average value: 4.05 GPa Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..