Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.10 - 5.60 GPa | 160 - 812 ksi | Average value: 2.03 GPa Grade Count:253 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 2.20 - 5.60 GPa | 319 - 812 ksi | Average value: 3.24 GPa Grade Count:5 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 3.59 - 5.60 GPa | 520 - 812 ksi | Average value: 4.86 GPa Grade Count:7 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |