Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.20 GPa | 319 ksi | ASTM D638 |
Network Polymers MS 150 IF Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Modulus of Elasticity | 2.20 - 2.50 GPa | 319 - 363 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_7210 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Modulus of Elasticity | 2.20 - 6.48 GPa | 319 - 940 ksi | Average value: 4.10 GPa Grade Count:62 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Modulus of Elasticity | 2.20 - 16.5 GPa | 319 - 2390 ksi | Average value: 5.74 GPa Grade Count:64 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50/TF/15/GY04 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50-7897 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50-8276 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 50-8300 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 80/TF/18/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 80-7318 Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 0104 Polycarbonate Suitable for extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 0407 Polycarbonate Suitable for extrusion, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 0712 Polycarbonate Suitable for molding and extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 1822 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D638 |
Iran Petrochemical (PCC) PC 2230 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ASTM D638 |
Wanshijie APET Sheet APET sheet is one of the earliest plastic sheets our company develops and produces. It has excellent air-tightness, durability, chemical resistance and transparency. When burnt, it will not produce .. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | ISO 527-2 |
Tisan TISREN® Flame Retardant (V0) Polystyrene TISREN has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimensio.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 21MB621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 25MB866 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side PVOH. It provides excellent gas and aroma protection and is designed to be use.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 26MB600 OPP Film Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 30MB666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Bicor™ 32MB768 OPP Film Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 2.20 GPa | 319 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2 K20 Nylon 6 High density and high modulusInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.20 - 2.80 GPa | 319 - 406 ksi | Average value: 2.54 GPa Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |