Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 50800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 350 GPa
50800 ksi
Plansee INERMET® IT176 Tungsten-Nickel-Copper Alloy
Characteristics:Non-MagneticEasy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive component..
Modulus of Elasticity 350 - 400 GPa
50800 - 58000 ksi
Young's modulus
Momentive Performance Materials Niobium Carbide (NbC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
Modulus of Elasticity 350 - 400 GPa
50800 - 58000 ksi
Young's modulus
Momentive Performance Materials Zirconium Carbide (ZrC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
Modulus of Elasticity 350 GPa
50800 ksi
Sapco 95% Aluminum Oxide
Information provided by Sapco.
Modulus of Elasticity 350 GPa
50800 ksi
Sapco 98% Aluminum Oxide
Information provided by Sapco.
Modulus of Elasticity 350 GPa
50800 ksi
ASTM E494
M Cubed Technologies SSC-702 Reaction-Bonded Silicon Carbide
Medium-grained reaction-bonded SiC for high wear applications. Bullnoses, fan liners, hydrocyclone liners, etc. Can be cast into very large shapes (greater than 4 ft. square, 5-6 inches thick)Info..
Modulus of Elasticity 350 GPa
50800 ksi
ASTM-C848
CoorsTek CAP 4 98.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Modulus of Elasticity 350 GPa
50800 ksi
ASTM-C848
CoorsTek FG-98 98% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Modulus of Elasticity 350 GPa
50800 ksi
ASTM C848
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Modulus of Elasticity 350 GPa
50800 ksi
Advanced Ceramics ACL 1091 (C-799) Alumina
Information provided by Advanced Ceramics Limited (ACL)
Modulus of Elasticity 350 GPa
50800 ksi
CeramTec Rubalit® A 1898 Alumina, 98%
Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..
Copyright © lookpolymers.com All Rights Reserved