Material Notes:
Information provided by Sapco.
Physical Properties Metric English Comments
Density 3.90 g/cc
0.141 lb/in³
Open Porosity 0.00 %
0.00 %
Weibull Modulus >= 10
>= 10
Mechanical Properties Metric English Comments
Hardness, Mohs 9.0
9.0
Tensile Strength, Ultimate 250 MPa
36300 psi
Modulus of Elasticity 350 GPa
50800 ksi
Flexural Strength 350 MPa
50800 psi
Compressive Strength 2600 MPa
377000 psi
Poissons Ratio 0.22
0.22
Shear Modulus 143 GPa
20700 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 8.20 µm/m-°C

@Temperature 20.0 °C
4.56 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.880 J/g-°C
0.210 BTU/lb-°F
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1700 °C
3090 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 9.2

@Frequency 1e+6 Hz
9.2

@Frequency 1e+6 Hz
Dielectric Strength 20.0 kV/mm
508 kV/in
AC
Dissipation Factor 0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
Dielectric Loss Index 0.0018
0.0018