Modulus of Elasticity 0.100 - 0.370 GPa
14.5 - 53.7 ksi
MetaFoam Copper Foam
General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional” metal foams. MetaFoam can ..
Modulus of Elasticity 0.100 - 0.370 GPa
14.5 - 53.7 ksi
MetaFoam Copper-Silver Foam
General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional” metal foams. MetaFoam can ..