Modulus of Elasticity 0.100 - 7.00 GPa
14.5 - 1020 ksi
Average value: 1.54 GPa Grade Count:94
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Modulus of Elasticity 0.100 - 0.370 GPa
14.5 - 53.7 ksi
MetaFoam Copper Foam
General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional” metal foams. MetaFoam can ..
Modulus of Elasticity 0.100 GPa
14.5 ksi
ASTM D638
ITW Plexus Plexusâ„¢ 3940 Methacrylate Adhesive
An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.Fast tacking, low pressure sprayable adhesive with long bonding range, ..
Modulus of Elasticity 0.100 - 0.370 GPa
14.5 - 53.7 ksi
MetaFoam Copper-Silver Foam
General Description:MetaFoam® Technologies intends to revolutionize the open-cell metal foams industry by alleviating the major constraints of “conventional” metal foams. MetaFoam can ..
Modulus of Elasticity 0.100 GPa
14.5 ksi
ISO 527-2
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi..
Modulus of Elasticity 0.100 - 3.30 GPa
14.5 - 479 ksi
Average value: 1.75 GPa Grade Count:25
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Modulus of Elasticity 0.100 - 13.0 GPa
14.5 - 1890 ksi
Average value: 1.50 GPa Grade Count:209
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..