Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0547 GPa | 7.93 ksi | ISO R527 |
Arkema Group Orevac® 9314 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Blown film coextrusionInformation provided by Arkema Group |