Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 71.7 GPa | 10400 ksi | |
Corning Large Cover Gorilla® Glass Touch Screen Glass Corning® Gorilla® Glass is a damage-resistant cover glass that is elegant, lightweight, and durable enough to resist many real-world events that commonly cause glass failure. The composition of C.. |
|||
Modulus of Elasticity | 71.7 GPa | 10400 ksi | |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |
|||
Modulus of Elasticity | 71.7 GPa | 10400 ksi | Fully Hardened |
ATI Wah Chang Tiadyne™ 3510 Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.Information provided by ATI Wah Chang |