Modulus of Elasticity >= 72.0 GPa
>= 10400 ksi
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Modulus of Elasticity 72.0 GPa
10400 ksi
Piezo Kinetics 406 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars. PKI 406 is suitabl..
Modulus of Elasticity 72.0 GPa
10400 ksi
Piezo Kinetics 802 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp..
Modulus of Elasticity >= 72.0 GPa
>= 10400 ksi
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4
High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Modulus of Elasticity 72.0 GPa
10400 ksi
Young's Modulus
Momentive Performance Materials Type 214 Fused Quartz Tubing
Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo..
Modulus of Elasticity 72.0 GPa
10400 ksi
Schott Glass 8516 Sealing Glass
Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
Modulus of Elasticity 72.0 GPa
10400 ksi
Schott LITHOSIL-Q Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 72.0 GPa
10400 ksi
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz
Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i..
Modulus of Elasticity 72.0 GPa
10400 ksi
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..
Modulus of Elasticity 72.0 GPa
10400 ksi
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Modulus of Elasticity 72.0 GPa
10400 ksi
tensile
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Modulus of Elasticity 72.0 GPa
10400 ksi
tensile
Constellium Alumold® 500 Forged Aluminum
Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to ..
Modulus of Elasticity 72.0 GPa
10400 ksi
tensile
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Modulus of Elasticity 72.0 GPa
10400 ksi
tensile
Constellium Certal® SPC Aluminum
Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man..
Modulus of Elasticity 72.0 GPa
10400 ksi
tensile
Constellium Certal® SPC Forged Aluminum
Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property..
Modulus of Elasticity 72.0 GPa
10400 ksi
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Modulus of Elasticity 72.0 GPa
10400 ksi
tensile
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Modulus of Elasticity 71.7 GPa
10400 ksi
Corning Large Cover Gorilla® Glass Touch Screen Glass
Corning® Gorilla® Glass is a damage-resistant cover glass that is elegant, lightweight, and durable enough to resist many real-world events that commonly cause glass failure. The composition of C..
Modulus of Elasticity 71.7 GPa
10400 ksi
Clinton Aluminum Alumold 1-500 Forged
Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is ..
Modulus of Elasticity 71.7 GPa
10400 ksi
Fully Hardened
ATI Wah Chang Tiadyne™ 3510
Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.Information provided by ATI Wah Chang