Mechanical Properties Metric English Comments
Modulus of Elasticity 5.17 - 17.9 GPa
750 - 2600 ksi
Average value: 8.75 GPa Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Modulus of Elasticity 5.17 - 13.1 GPa
750 - 1900 ksi
Average value: 8.41 GPa Grade Count:10
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim..
Modulus of Elasticity 5.17 GPa
750 ksi
ASTM D638
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey
Information provided by ITW Devcon
Modulus of Elasticity 5.17 GPa
750 ksi
ASTM D638
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey
Information provided by ITW Devcon
Modulus of Elasticity 5.17 GPa
750 ksi
In Tension; ASTM D638
Devcon Underwater Repair Putty (UW) Epoxy
Emergency Repair ProductsComments: High-performance technology for repairing, patching and rebuilding equipment in habitually wet environments, even under water. Eliminates the need for substrate t..
Modulus of Elasticity 5.17 GPa
750 ksi
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% ..
Modulus of Elasticity 5.17 GPa
750 ksi
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°..