Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0650 GPa
9.43 ksi
ISO 527-2
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt..
Modulus of Elasticity 0.0650 GPa
9.43 ksi
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...