Polymer Property : Modulus of Elasticity = 9.65 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.10 - 9.65 GPa
450 - 1400 ksi
Average value: 6.00 GPa Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu..
Modulus of Elasticity 1.06 - 9.65 GPa
154 - 1400 ksi
Average value: 2.83 GPa Grade Count:311
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Modulus of Elasticity 5.00 - 9.65 GPa
725 - 1400 ksi
Average value: 7.89 GPa Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Modulus of Elasticity 1.65 - 9.65 GPa
240 - 1400 ksi
Average value: 4.09 GPa Grade Count:21
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max..