Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.627 GPa | 90.9 ksi | Molded Sample 2% Secant Modulus |
Dow HDPE 38152M High Density Polyethylene DOW HDPE 38152M resin is a medium molecular weight distribution copolymer designed to offer good impact strength and stress crack resistance with excellent toughness. This resin has excellent proces.. |