Fatigue Strength 303 MPa

@# of Cycles 100000
44000 psi

@# of Cycles 100000
Smooth
Alcoa 2090-T83 Aluminum
Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has ..