Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 303 MPa @# of Cycles 100000 |
44000 psi @# of Cycles 100000 |
Smooth |
Alcoa 2090-T83 Aluminum Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has .. |