Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 14.0 J | 10.3 ft-lb | Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C |
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe.. |
|||
Charpy Impact | 14.0 J | 10.3 ft-lb | Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C |
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b.. |
|||
Charpy Impact | 14.0 J @Temperature -73.0 °C |
10.3 ft-lb @Temperature -99.4 °F |
V-Notch |
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |