Charpy Impact 14.0 J
10.3 ft-lb
Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel
Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe..
Charpy Impact 14.0 J
10.3 ft-lb
Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel
Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b..
Charpy Impact 14.0 J

@Temperature -73.0 °C
10.3 ft-lb

@Temperature -99.4 °F
V-Notch
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..