Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact = 11.1 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 15.0 J
11.1 ft-lb
Typical (Transverse)
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T..
Charpy Impact 15.0 J

@Temperature -20.0 °C
11.1 ft-lb

@Temperature -4.00 °F
Typical (Longitudinal)
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T..
Charpy Impact 15.0 J
11.1 ft-lb
Industeel Superplast® 350 Mold Steel
SUPERPLAST® 350 offers improved machinability, improved consistency and weldability, improved thermal conductivity, with a higher hardness allowing better mechanical properties and polishability...
Charpy Impact 15.0 J
11.1 ft-lb
Haynes 625 alloy, plate after 1000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 15.0 J
11.1 ft-lb
Haynes 625 alloy, plate after 4000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 15.0 J
11.1 ft-lb
50% cold rolled and 500 hours at 500°C (930°F)
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Charpy Impact 15.0 J

@Temperature -40.0 °C
11.1 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp SECURE 500 Structural Steel
This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 500 for civil use, that is usually produced in thickness from 3 mm up to 90 mm.App..
Charpy Impact 15.0 J

@Temperature -40.0 °C
11.1 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp SECURE 600 Structural Steel
This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 600 for civil use, that is usually produced from 4 up to 40 mm in thickness.Applic..
Charpy Impact 15.0 J
11.1 ft-lb
tempering at 450°C (842°F). Hardened at 960°C (1760°F). Quenched in air. Tempered twice.
Assab Steels CALMAX Plastic Mold Material
CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo..
Copyright © lookpolymers.com All Rights Reserved