Mechanical Properties Metric English Comments
Charpy Impact 7.00 - 15.0 J
5.16 - 11.1 ft-lb
Notched; after age hardening
EOS MS1 Maraging Steel for DMLS 3D Printing
EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us..