Polymer Property : Charpy Impact = 7.00 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 7.00 J
5.16 ft-lb
Haynes 625 alloy, plate after 1000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 7.00 J
5.16 ft-lb
Haynes 625 alloy, plate after 8000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 7.00 J
5.16 ft-lb
Haynes 625 alloy, plate after 8000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 7.00 - 15.0 J
5.16 - 11.1 ft-lb
Notched; after age hardening
EOS MS1 Maraging Steel for DMLS 3D Printing
EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us..
Charpy Impact 7.00 J

@Temperature -196 °C
5.16 ft-lb

@Temperature -321 °F
V-notch
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..