Polymer Property : Charpy Impact = 5.00 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 6.78 J
5.00 ft-lb
Notched
Schmolz + Bickenbach MoldMAX® V Copper Alloy
Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores ..
Charpy Impact 6.78 J
5.00 ft-lb
Gray iron usually not recommended in high impact loading applications
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i..
Charpy Impact 6.78 J
5.00 ft-lb
hardened at 2175°F; C-notch
Crucible Steel REX® M42 High Speed Steel, AISI M42
REX M42 is a super cobalt high speed steel which may be heat treated to HRC 68. This makes REX M42 outstanding for special purpose cutting tools, with requirements beyond the capability of general p..
Charpy Impact 6.78 J
5.00 ft-lb
V-Notch; Oil Quenched from 816°C for 4 hours; 316°C Temper Temperature
Latrobe LSS™ L6 Tool Steel (ASTM L6)
TLS L6 tool steel is a versatile, oil-hardening tool steel that is characterized by very good toughness. TLS L6 tool steel is suitable for use as tools, dies, and machine parts which require a good ..