Material Notes:
TLS L6 tool steel is a versatile, oil-hardening tool steel that is characterized by very good toughness. TLS L6 tool steel is suitable for use as tools, dies, and machine parts which require a good combination of hardness and toughness. The relatively high nickel content results in an alloy with greater impact toughness compared to the other common oil-hardening grades. Typical applications for TLS L6 tool steel include punches and dies, cold forming tools, and coining dies.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.86 g/cc
7.86 g/cc
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 62
62
Air Cooled from 760°C, 30 minutes
63.5
63.5
Air Cooled from 788°C, 30 minutes
63.5
63.5
Air Cooled from 843°C, 30 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 75 %
75 %
1% Carbon Steel
Charpy Impact 1.36 J
1.00 ft-lb
V-Notch; Oil Quenched from 816°C for 4 hours; 150°C Temper Temperature
4.75 J
3.50 ft-lb
V-Notch; Oil Quenched from 816°C for 4 hours; 205°C Temper Temperature
6.78 J
5.00 ft-lb
V-Notch; Oil Quenched from 816°C for 4 hours; 316°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 11.81 µm/m-°C

@Temperature 21.0 - 149 °C
6.561 µin/in-°F

@Temperature 69.8 - 300 °F
14.36 µm/m-°C

@Temperature 21.0 - 538 °C
7.978 µin/in-°F

@Temperature 69.8 - 1000 °F
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 0.70 %
0.70 %
Chromium, Cr 0.70 %
0.70 %
Iron, Fe 96.35 %
96.35 %
Manganese, Mn 0.60 %
0.60 %
Nickel, Ni 1.4 %
1.4 %
Silicon, Si 0.25 %
0.25 %
Chemical Properties Metric English Comments
Critical Temperature 719 °C
1330 °F
Ac1