Mechanical Properties Metric English Comments
Charpy Impact 63.0 J
46.5 ft-lb
Hardening Temperature- 1120°C; Tempering Temperature- 540°C
Crucible Steel CPM® 9V® Tool Steel
CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced..