Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.235 GPa
34.1 ksi
12.7mm/min; ASTM D790
Westlake EC4042AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4042 is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combi..