Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tangent Modulus | 740 - 1590 MPa | 107000 - 230000 psi | Average value: 1250 MPa Grade Count:10 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |