Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tangent Modulus | 1104 MPa | 160100 psi | ASTM D790 |
Flint Hills AP6835-HS Polypropylene Impact Copolymer Features: Excellent processing, good low temperature impact strength.Applications: Injection molding: Appliance components, consumer durables and closuresInformation Provided by Flint Hills Resource.. |