Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills AP6835-HS Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills AP6835-HS Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent processing, good low temperature impact strength.Applications: Injection molding: Appliance components, consumer durables and closuresInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 91
91
ASTM D785
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Izod Impact, Notched 1.53 J/cm

@Temperature 23.0 °C
2.87 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 1104 MPa
160100 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Users viewing this material also viewed the following: