Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 7.17 MPa | 1040 psi | to Oriented Polypropylene (OPP) @ 550°F, 1.0 mil coating onto 50 lb Kraft paper; Dow Method |
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ult.. |