Adhesive Bond Strength 7.93 MPa
1150 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 724-9 Polyurethane Adhesive
TRA-BOND 724-9 premixed and frozen polyurethane adhesive has excellent adhesion and provides strong resilient bonds to a wide variety of substrates including aluminum, solder, nylon, mylar and steel..