Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 12.3 MPa | 1790 psi | ASTM D-229 |
Glastic T-160 Fiberglass-Reinforced Polyester Laminate Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load.. |