Polymer Property : Adhesive Bond Strength = 14.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 14.1 MPa
2050 psi
Polyester-Polyester; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..
Adhesive Bond Strength 14.1 MPa

@Temperature -54.4 °C
2050 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-2/A Epoxy Adhesive
This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac..
Adhesive Bond Strength 14.1 MPa

@Temperature 25.0 °C
2050 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-5/A Epoxy Adhesive
Information provided by Ellsworth Adhesives.
Adhesive Bond Strength 14.1 MPa

@Temperature 25.0 °C
2050 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong C-7/H20 Epoxy Adhesive
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..
Adhesive Bond Strength 14.1 MPa

@Temperature -54.4 °C
2050 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong X-81-A/F Epoxy Adhesive
Information provided by Ellsworth Adhesives.